Salve, di seguito la risposta di Jefa riguardo la mia domanda sulla tolleranza della profondità della corrosione. Io la ritengo una parte vitale e quindi l'ho sostituito.
Sul forum Hanse trovi decine di messaggi a riguardo.
Ogg: RE: Advice on rudderstock condition
To try and make a general rule, we suggest pitting corrosion should not be deeper than 1,5-2mm.
This, because many stocks will no longer pass ISO12215 if their diameter is reduced by that much. No doubt you already know the possible causes, but our resource on corrosion may be of assistance, https://jefa.com/install/electro.htm .
Sul forum Hanse trovi decine di messaggi a riguardo.
Ogg: RE: Advice on rudderstock condition
To try and make a general rule, we suggest pitting corrosion should not be deeper than 1,5-2mm.